Introduction
PET preforms are semi-finished products for blow molding. Moisture absorption is the most common hidden risk for PET materials. Once the moisture content of preforms exceeds the standard, silver streaks, bubbles, whitening and reduced bottle strength will appear during blow molding, which directly affects the quality of finished plastic bottles. This article covers standard PET preform storage conditions, moisture absorption principles, and practical operation methods to help factories and buyers avoid defective blow molded products.
What Causes PET Preform Moisture Absorption?
PET is a hygroscopic polymer material that continuously absorbs water vapor from the air at room temperature. After injection molding, the macromolecules inside PET preforms absorb moisture. When the moisture content exceeds the critical value (generally greater than 0.05%), the water will vaporize during the heating stage of blow molding, forming bubbles and silver streaks inside the bottle.
Ambient temperature and humidity are core factors affecting water absorption speed. Higher humidity accelerates preform moisture absorption, and higher temperature also speeds up this reaction. Exposed PET preforms can exceed the moisture limit within just a few days and become unsuitable for blow molding.
Recommended PET Preform Storage Conditions
1. Ambient Temperature & Relative Humidity
Ideal storage environment: temperature 15~25°C, relative humidity RH <40%.
When warehouse humidity stays above 50% for a long time, PET preforms absorb moisture rapidly. Extra dehumidification is required in coastal areas and rainy seasons.
2. Packaging Requirements for Preforms
Freshly molded PET preforms must be fully cooled down to room temperature, then sealed immediately in aluminum foil moisture-proof bags with desiccants inside.
Packaging bags should remain intact. Any tear or leak will break the moisture protection and expose preforms to humid air. Stacked cartons should not directly touch walls or floors to prevent moisture seepage.
3. Storage Stacking & Shelf Life
Well-sealed PET preforms can be stored for up to 6 months under standard warehouse temperature and humidity.
Do not stack cartons too high to avoid deformation of bottom boxes. Manage batches strictly and follow the first-in, first-out rule to use older preforms first.
How to Avoid Moisture Damage Before Blow Molding
1. Check Package Integrity Before Use
Inspect the moisture barrier bag for tears or air leakage before opening. If packaging is damaged, test preform moisture content and confirm it meets requirements before blow molding.
2. Drying Treatment for Moist Preforms
Preforms that have absorbed moisture must be dried. Standard drying parameters: 160~170°C for 4~6 hours, to reduce moisture content below 0.04%. After drying, send preforms to blow molding machine as soon as possible, do not leave them exposed to air and reabsorb moisture.
3. Control Exposure Time After Opening Bags
After opening the moisture-proof bag, use up all preforms within 4 hours. Opened preforms left in humid workshop air will quickly re-absorb moisture, even if they have been dried previously.
Common Defects Caused by Wet PET Preforms
Blow molding with wet PET preforms will create typical defects: silver streaks, tiny bubbles, whitening on transparent bottles. Finished bottles will have lower internal pressure resistance and are prone to leakage. This creates a risk of bottle rupture, especially for food packaging filled with edible oil or sauce.
FAQ
Q1: Can PET preforms be stored in a regular warehouse without a dehumidifier?
A: Only if your local climate stays dry and RH keeps below 40%. For humid coastal regions or rainy seasons, a dehumidifier is mandatory, otherwise preforms will quickly absorb moisture.
Q2: What is the safe moisture content for PET preforms before blow molding?
A: The standard safe moisture level is less than 0.05%. For food-grade plastic bottles, we recommend keeping moisture under 0.04%.
Q3: How long can PET preforms stay exposed after opening the moisture barrier bag?
A: We recommend using all opened preforms within 4 hours. Longer exposure causes re-absorption of moisture and blow molding defects.
Q4: Do sealed PET preforms still need drying before blow molding?
A: If the aluminum foil bag remains intact and stored under proper conditions, extra drying is not required. Always test moisture if packaging is damaged.